Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Multibase Nylex™ 4032 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Total 819E Polystyrene
(discontinued **) Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Edgetek® AT-20GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | Max Load; ASTM D790 |
Spartech PP5410 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES Luriblend® PA4/6 TL15 HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ecomass® 1003ZD95 Tungsten Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ensinger Tecatron® XP-88 Compression Molded PPS Compound, with 10% Graphite, 15% PTFE and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Cast Nylons Nycast® 12 Cast Nylon 12 NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | |
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell.. |
|||
Flexural Strength | 62.1 - 82.7 MPa | 9000 - 12000 psi | |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Flexural Strength | 62.1 - 89.6 MPa | 9000 - 13000 psi | |
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | |
BCC Products BC 7053 Epoxy Casting BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Edgetek® AT-30GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation. |
|||
Flexural Strength | >= 62.1 MPa | >= 9000 psi | |
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to.. |