Mechanical Properties Metric English Comments
Flexural Strength 297 MPa
43100 psi
ASTM D-790
PlastiComp Complet® LCF30-PPS Polyphenylene Sulfide, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphenylene Sulfide with 30% long carbon fiber reinforcementInformation provided by ..
Flexural Strength 297 MPa
43100 psi
ASTM D-790
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by..
Flexural Strength 297 MPa
43100 psi
ASTM D790
PlastiComp Complet® LGF40-PA66 MT 40% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Flexural Strength 297 MPa
43100 psi
SGL Carbon Group SIGRAFIL C® filled PEEK
Information provided by SGL Carbon Group
Flexural Strength 297 MPa
43100 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..
Flexural Strength 297 MPa
43100 psi
ASTM D790
Techmer ES HiFill® PA6 GF33 HS L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Heat Stabilized, Good UV..
Flexural Strength 297 MPa
43100 psi
ASTM D790
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearanc..
Flexural Strength 297 MPa
43100 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF007SXQ PA 66
LNP THERMOCOMP* RF007SXQ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Hydrolysis Resistant.
Flexural Strength 297 MPa
43100 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66
LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Strength 297 MPa
43100 psi
ISO 178
SABIC Innovative Plastics LNP VERTON PV007 PA 6
LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural.
Flexural Strength 297 MPa
43100 psi
ASTM Test
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Flexural Strength 297 MPa

@Temperature -40.0 °C
43100 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Flexural Strength 297 MPa
43100 psi
ISO 178
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific)
LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber.
Flexural Strength 297 MPa
43100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP VERTON RX00327 PA 66
LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural.
Copyright © lookpolymers.com All Rights Reserved