Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 240 MPa | 34800 psi | |
Plastcom SLOVAMID 66 GF 30 HI PA66, 30% glass fibre, improved strength FeaturesPA 66 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength .. |
|||
Flexural Strength | 240 MPa | 34800 psi | ISO 178 |
Nilit FRIANYL A63 TF-GV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical.. |
|||
Flexural Strength | <= 240 MPa | <= 34800 psi | ISO 178 |
Polykemi AB SCANMID 6 B12^ QF2010 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 240 MPa | <= 34800 psi | ISO 178 |
Polykemi AB SCANMID 6 B13^ F30 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 240 MPa | 34800 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Flexural Strength | 240 MPa | 34800 psi | |
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Flexural Strength | 240 MPa | 34800 psi | |
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Flexural Strength | 240 MPa | 34800 psi | |
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Flexural Strength | 240 MPa | 34800 psi | ASTM D790 |
Kuraray Genestarâ„¢ GN2330 Nylon, 33% Glass Filled Standard V-0 Grade. Features a balance of mechanical strength, mold-ability, and dimensional stability. Well suited for a wide range of electrical and electronic components. |
|||
Flexural Strength | 240 MPa | 34800 psi | ASTM D790 |
Kuraray Genestarâ„¢ GT2330 Nylon, 33% Glass Filled Toughness V-0 Grade. It is well suited for components requiring a high strength in pin fitting process, due to high ductility properties. |
|||
Flexural Strength | 240 MPa | 34800 psi | ASTM D790 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Flexural Strength | 240 MPa | 34800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Flexural Strength | 240 MPa | 34800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Flexural Strength | 240 MPa | 34800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Flexural Strength | 240 MPa | 34800 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Flexural Strength | 240 MPa | 34800 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EF004 PEI LNP* Thermocomp* EF004 is a compound based on Polyetherimide resin containing 20% Glass Fiber. |
|||
Flexural Strength | 240 MPa | 34800 psi | ISO 178 |
Polyram RamLloy A300NT Nylon 66/Polypropylene Alloy, 30% Glass Fiber Reinforced Nylon 66/PP alloy 30% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 240 MPa | 34800 psi | ISO 178-93 |
Wellman Wellamid® GFX1717-BK1 Nylon 66, 43% Glass Fiber Reinforced, Silicone Lubricated All information provided by Wellman Engineered Resins. |
|||
Flexural Strength | 240 MPa | 34800 psi | ASTM D790 |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Flexural Strength | >= 240 MPa | >= 34800 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe. |
|||
Flexural Strength | 240 MPa | 34800 psi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Flexural Strength | 240 MPa | 34800 psi | ISO 178 |
Eurotec® Tecomid® NB40 GR30 NL PA 6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Strength | 240 MPa | 34800 psi | ISO 178 |
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Flexural Strength | 240 MPa | 34800 psi | ASTM Test |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Flexural Strength | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |