Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 30200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 208 MPa
30200 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS
LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Flexural Strength 208 MPa
30200 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF008E PES
LNP* THERMOCOMP* JF008E is a compound based on Polyethersulfone containing 40% Glass Fiber. Characteristics of this grade are: Easy Molding.
Flexural Strength 208 MPa
30200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT
LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber.
Flexural Strength 208 MPa
30200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10
LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Strength 208 MPa
30200 psi
2 mm/min; ISO 178
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber
SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme..
Flexural Strength 208 MPa
30200 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp XF006S
LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region..
Flexural Strength 208 MPa
30200 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA
LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized.
Flexural Strength 208 MPa
30200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific)
LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Strength 208 MPa
30200 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 442 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Strength 208 MPa
30200 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 622 Nylon 6/6, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Copyright © lookpolymers.com All Rights Reserved