Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Asia Pacific) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Europe-Africa-Middle East) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N1320HL BK Post Consumer Recycle Nylon 66, 20% Glass Filled Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 168 MPa | 24400 psi | Bending s<sub>bB</sub>; DIN EN 1288, Part 5, R45 |
Schott Nextrema® 712-3 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ZFL36CCX PPE+PS LNP LUBRICOMP* ZFL36CCX is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater.. |
|||
Flexural Strength | 168 MPa | 24400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RE004MPC PA 66 LNP* STAT-KON* RE004MPC is a compound based on Nylon 66 resin containing 20% Milled Carbon Fiber. Added features of this material are: Exceptional Processing, Clean Compound System, Electrically C.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific) LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF002E PES (Asia Pacific) LNP THERMOCOMP* JF002E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ISO 178 |
Polyplastics Duranex® 7307 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 168 MPa | 24400 psi | ISO 178 |
Polyplastics FR-PET® C3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Strength | 168 MPa | 24400 psi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |
|||
Flexural Strength | 168 MPa | 24400 psi | GB/9341 |
Zhejiang Juner PA66-301-G20 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Framework of CoilsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 168 MPa | 24400 psi | ISO 178 |
Polyplastics FR-PET® B3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Strength | 168 MPa | 24400 psi | ISO 178 |
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic Vyncolit A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Strength | 168 MPa | 24400 psi | ISO 178 |
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled) AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu.. |
|||
Flexural Strength | 168 MPa @Temperature -40.0 °C |
24400 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8202C HS PA6 (Conditioned) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Flexural Strength | 168 MPa @Temperature -40.0 °C |
24400 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8202C PA6 (Conditioned) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Flexural Strength | 168 MPa @Temperature -40.0 °C |
24400 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D790 |
Beijing Ranger Chem PBT-MFC-G20 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Strength | 168 MPa | 24400 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF002E PES LNP THERMOCOMP* JF002E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the America.. |