Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 146 MPa | 21200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS PC+ABS Blend with 20% Glass Reinforce. High heat resistance; Excellent balance strength/rigidity; Good impact/appearance. |
|||
Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC (Asia Pacific) LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Flexural Strength | <= 146 MPa | <= 21200 psi | ISO 178 |
Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant Information provided by Polykemi AB |
|||
Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Flexural Strength | 146 MPa @Temperature 22.0 °C |
21200 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp GFL14 PSU LNP* Lubricomp* GFL14 is a compound based on Polysulfone containing Glass Fiber and PTFE Lubricant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 146 MPa | 21200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK) KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry .. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Strength | 146 MPa | 21200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
Azdel Plus C401-B01 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Flexural Strength | 146 MPa | 21200 psi | ASTM D790 |
Asahi Kasei Thermylene® P-40FG-0860 40% Glass Fiber Reinforced Information provided by Asahi Thermofil |