Mechanical Properties Metric English Comments
Flexural Strength 116 MPa
16800 psi
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data)
This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin..
Flexural Strength 116 MPa
16800 psi
ASTM D790
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Strength 116 MPa
16800 psi
ASTM D790
Nilit Polynil® P60 Medium Viscosity Nylon 66
Description: Polynil P60 is a grade has a viscosity that has been optimized for monofilament extrusion.Key characteristics: Viscosity number 155 gr/cm3Excellent melt stabilityHigh elongationInformat..
Flexural Strength 116 MPa
16800 psi
ASTM D790
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)  (Unverified Data**)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E..
Flexural Strength 116 MPa
16800 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0001 PC
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Strength 116 MPa
16800 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Flexural Strength 116 MPa
16800 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Flexural Strength 116 MPa
16800 psi
ASTM D790
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491..
Flexural Strength 116 MPa
16800 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® GR-4017 ABS, Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Strength 116 MPa
16800 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® GR-4017 ABS, Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Strength 116 MPa
16800 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12
LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare
Flexural Strength 116 MPa
16800 psi
ASTM D790
Techmer ES Luriblend® POM CO AF15
Availability: North AmericaForms: PelletsAdditive: Aramid Resin Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc.
Flexural Strength 116 MPa
16800 psi
ASTM D790
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
Flexural Strength 116 MPa
16800 psi
ASTM D638
Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..
Flexural Strength 116 MPa
16800 psi
ASTM D790
Plenco 6401 Phenolic, Granular, Compression Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Flexural Strength 116 MPa
16800 psi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
Flexural Strength 116 MPa
16800 psi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
Flexural Strength 116 MPa
16800 psi
GB/9341
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66
Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Flexural Strength 116 MPa
16800 psi
ISO 178
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Flexural Strength 116 MPa
16800 psi
ASTM D790
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced
Information provided by Entec
Flexural Strength 116 MPa
16800 psi
ISO 178
Azoty Tarnow™ TARNOFORM 300 GF3 POM
15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Flexural Strength 116 MPa
16800 psi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-0153 30% Glass Fiber Reinforced, Chemically Coupled
Information provided by Asahi Thermofil
Flexural Strength 116 MPa
16800 psi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-0570 30% Glass Fiber Reinforced, Flame Retardant
Information provided by Asahi Thermofil
Flexural Strength 116 MPa
16800 psi
ASTM D790
Ashley Polymers Ashlene® N541 Nylon 66
A general purpose high viscosity extrusion grade Nylon 66 with very good natural color.Data provided by the manufacturer
Flexural Strength 116 MPa
16800 psi
ASTM D790
Ashley Polymers Ashlene® N541L Nylon 66
A general purpose injection molding grade for heavy parts.Data provided by the manufacturer
Flexural Strength 116 - 143 MPa
16800 - 20800 psi
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound
BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr..
Flexural Strength 116 MPa
16800 psi
2 mm/min; ISO 178
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000
PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me..