Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 100 MPa | 14500 psi | STN EN ISO 178 |
Plastcom PLASTAMID® 66 BT B 27 A/IM PA66 Basic type PA66 for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fas.. |
|||
Flexural Strength | 100 MPa | 14500 psi | ISO 178 |
Nilit FRIANYL A63 HS-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | <= 100 MPa | <= 14500 psi | ISO 178 |
Polykemi AB SCANTEC PC S60R Polycarbonate Information provided by Polykemi AB |
|||
Flexural Strength | 100 MPa @Temperature 23.0 °C |
14500 psi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | <= 100 MPa | <= 14500 psi | ISO 178 |
Polykemi AB SCANTEC PC S75R Polycarbonate Information provided by Polykemi AB |
|||
Flexural Strength | 100 MPa | 14500 psi | Molded; ASTM D790 |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Flexural Strength | 100 MPa | 14500 psi | Molded; ASTM D790 |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Flexural Strength | 100 MPa | 14500 psi | |
ICE Mullite, 3Al2O3-SiO2 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Flexural Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Strength | 100 MPa | 14500 psi | ISO 178 |
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec.. |
|||
Flexural Strength | 100 MPa | 14500 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 100 MPa | 14500 psi | GB/T 9341-2008 |
Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide Injection molding, reinforcedInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Strength | 100 MPa | 14500 psi | 2mm/min; ISO 178 |
Teijin Multilon DN-3520F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high flowability realizes a thin w.. |
|||
Flexural Strength | 100 MPa | 14500 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PH0390A PA 6 LNP THERMOCOMP* PH0390A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 100 MPa | 14500 psi | 2.0 mm/min (3 point); ISO 178 |
Styron CALIBREâ„¢ 703-15 Polycarbonate Resin Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce.. |
|||
Flexural Strength | 100 MPa | 14500 psi | ASTM D790 |
Styron EMERGEâ„¢ 4600-10 Polycarbonate EMERGEâ„¢ PC 4600-10 advanced resin is formulated to supply both clarity and enhanced ignition resistance while maintaining excellent physical properties. Applications: Information Technology E.. |
|||
Flexural Strength | 100 MPa | 14500 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 100 MPa | 14500 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific) LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 100 MPa | 14500 psi | ASTM D790 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Flexural Strength | 100 MPa | 14500 psi | ISO 178 |
Polyram RamOfin PPH501G4 Polypropylene, 20% Glass Fiber, Flame Retardant Glass fiber 20% reinforced, halogen free, flame retardant polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 100 MPa | 14500 psi | ISO 178 |
Polyram RamTough PZ126 Polycarbonate, Low Viscosity General purpose, low viscosity polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | >= 100 MPa @Diameter >=100 mm |
>= 14500 psi @Diameter >=3.94 in |
Perpendicular to laminations; IEC 1212-2 4.1 |
Hippe PF CP 22 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube High-voltage, electrical applications at power frequencies. High electric strength in oil.Information provided by Hippe. |
|||
Flexural Strength | 100 MPa | 14500 psi | ASTM D790 |
Aclo Accucomp Polycarbonate POL050L Low Viscosity |
|||
Flexural Strength | 100 MPa @Temperature 93.0 °C |
14500 psi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Flexural Strength | <= 100 MPa | <= 14500 psi | cond., 3.5% flexure; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |