Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Quadrant EPP Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet) |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0266 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 1020 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D 790 |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0254 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0348 Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0390 S1 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® POM 0212B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Chase Plastics CP Pryme® PE-200-HD8M General Purpose High Density Polyethylene Information provided by Chase Plastics. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Ecomass® 1050ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyGood ToughnessInformation provided by Technical Polymers |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Ensinger Tecaform™ SD Acetal (POM) Ensinger-Hyde static dissipative acetal contains no carbon fibers or powders and is generally accepted for clean room use. With its surface resistivity of 109 to 1011 ohm/square and its excellent b.. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | |
3M Scotchkote™ FG 502 Epoxy Metal Repair Scotchkote Epoxy Metal Repair FG 502 has been specifically developed as a 100% solids epoxy coating for resurfacing and reforming metal machinery and equipment. It also combines good application cha.. |
|||
Flexural Strength | 48.3 MPa | 7010 psi | ASTM D790 |
Adell EA-16 Homopolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Asahi Kasei Thermofil P-20TC-5103 20% Talc Reinforced, Lubricated, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Asahi Kasei Thermofil P-20TC-Y118 20% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Asahi Kasei Thermofil P-40MI-0600 40% Mica Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 48.3 MPa | 7010 psi | ASTM D790 |
Adell RQ-18 Copolymer Polypropylene, 40% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA12 1100 Tungsten Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Tungsten FillerInformation provided by TP Composites, Inc. |