| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Adell RQ-18 Copolymer Polypropylene, 40% Mica Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.235 g/cc | 0.04462 lb/in³ | ASTM D792 |
| Water Absorption | 0.040 % | 0.040 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 70 | 70 | ASTM D785 |
| Hardness, Rockwell R | 100 | 100 | ASTM D785 |
| Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Flexural Strength | 48.3 MPa | 7010 psi | ASTM D790 |
| Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
| Gardner Impact | 1.10 J | 0.811 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 160 °C | 320 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 141 °C | 286 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |