Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 270 MPa | 39200 psi | |
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Nilit FRIANYL A63 W-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
DSM Akulon® K-FG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
DSM Akulon® K-FHG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Flexural Strength | 270 MPa | 39200 psi | |
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynam.. |
|||
Flexural Strength | 270 MPa | 39200 psi | |
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
Flexural Strength | 270 MPa | 39200 psi | |
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
Flexural Strength | 270 MPa | 39200 psi | 5 mm/min; ISO 178 |
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 270 MPa | 39200 psi | 5 mm/min; ISO 178 |
Gromax BFG30-FH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 270 MPa | 39200 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 (Asia Pacific) LNP LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Flexural Strength | 270 MPa | 39200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific) LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Flexural Strength | 270 MPa | 39200 psi | dry; ISO 178 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
DSM Akulon® Ultraflow™ K-FHG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Strength | 270 MPa | 39200 psi | Longitudinal direction; ISO 178 |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |
|||
Flexural Strength | <= 270 MPa | <= 39200 psi | ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, Conditioned Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Flexural Strength | 270 MPa | 39200 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Strength | 270 MPa @Temperature 23.0 °C |
39200 psi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe |
|||
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |