Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Strength | 27.6 MPa | 4000 psi | 13 mm/min; ASTM D790 |
PolyOne Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Oxford Polymers PC 20 Unfilled Polycarbonate for Injection Molding Unfilled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Niche Polymer PPCM10BK Copolymer PP Information provided by Niche Polymer |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Niche Polymer PPCM15BK Copolymer PP Information provided by Niche Polymer |
|||
Flexural Strength | 27.6 MPa | 4000 psi | |
Pyrotek ISOMAG® 175 Structural Insulation Board Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Network Polymers 707 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Flexural Strength | 27.6 MPa | 4000 psi | Conditioned; ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
I. Stern 550 High Impact Polystyrene Features:Good process propertiesExcellent toughness and environmental stress crackingApplicationsStructural foamDisplaysSmall appliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Informat.. |
|||
Flexural Strength | 27.6 MPa @Temperature 260 °C |
4000 psi @Temperature 500 °F |
|
Greene Tweed Arlon® 2000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Techmer ES Statiblend® 02010 MB Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinfor.Features: ConductiveAppearance: BlackTPCI# 9125116Information provided by TP Composites, Inc. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Techmer ES HiFill FR® HIPS FR V-2 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Westlake Plastics Propylux® CN-P Polypropylene (conductive) Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Chesterton MRS S4+ Metal Rebuilding System An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 .. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D-790 |
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board REN Shape 450 is the preferred modeling board for pattern makers throughout the world. The outstanding dimensional stability and its ability to hold precise tolerances even after exposure to heat h.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | |
Abatron ROCKWELD 55-27 A/B Structural Adhesive Putty; Epoxy ROCKWELD 55-27 is a 2-component epoxy system with low density, high-strength, and no shrinkage. It is a structural adhesive putty for sculpturing, repairs and restoration of stone, concrete and maso.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | |
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required. |
|||
Flexural Strength | 27.6 MPa @Temperature 150 °C |
4000 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Chesterton ARC S4+ 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375.. |