Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding 33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Strength | 269 MPa | 39000 psi | |
Premix Premi-Glas® 1200-50VE 1200-50 VE SMC
(discontinued **) Description: Premi-Glas® 1200-50 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Flexural Strength | 269 MPa | 39000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF33 TL15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP C.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF43 ML2 BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated Appearance: BlackTPCI# 8047101Informa.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES Luriblend® PPA CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 269 MPa | 39000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 269 MPa | 39000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Chase Plastics CP Pryme® N130GL (DAM) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 269 MPa @Temperature 23.0 °C |
39000 psi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 269 MPa @Temperature 23.0 °C |
39000 psi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |