Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Radici Radilon® SRV300 (dry) Nylon 6 Glass-fiber reinforcedInformation provided by Radici group. |
|||
Flexural Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Flexural Strength | 250 MPa | 36300 psi | |
Lehmann & Voss LUVOCOM® 1105-7920/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Flexural Strength | >= 250 MPa | >= 36300 psi | |
Hybrid Plastics Fireban® Mark VI-IS Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Grupo Repol Dinalon® A1S25 G35PV0 35% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled 30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
Flexural Strength | 250 MPa | 36300 psi | |
Lehmann & Voss LUVOCOM® 1-1108 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Flexural Strength | 250 MPa | 36300 psi | 3.5%; ISO 178 |
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
Flexural Strength | 250 MPa | 36300 psi | 5 mm/min; ISO 178 |
Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 250 MPa | 36300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REF42XXP PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* REF42XXP is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI LNP* THERMOCOMP* EC004XXC is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI (Asia Pacific) LNP* Thermocomp* EC004XXC is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific) LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Strength | 250 - 300 MPa | 36300 - 43500 psi | At Rupture; ISO 178 |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ASTM-D790 |
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178-93 |
Wellman Wellamid® GF33-66/6 XE-BKDX9 Nylon 66/6, 33% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Flexural Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® 4000 Mold Insulation Material Insulation of clamping platesInformation provided by elisto |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Strength | 250 MPa | 36300 psi | cond; ISO 178 |
DSM EcoPaXX® Q-HG10 PA410-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |