Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 157 MPa | 22800 psi | ASTM D-790 |
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D-790 |
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
Kolon KOCETAL® GF305 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
Haysite H330 Polyester Composite A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ.. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp OFP36A PPS - Branched (Asia Pacific) LNP LUBRICOMP* OFP36A is a compound based on PPS - Branched resin containing Silicone, PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.This data was supplied by SA.. |
|||
Flexural Strength | 157 MPa | 22800 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Flexural Strength | 157 MPa | 22800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 157 MPa | 22800 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-4240 PPS/PPA Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 157 MPa | 22800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 157 MPa | 22800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP OF008G PPS - LINEAR LNP* THERMOCOMP* OF008G is a compound based on PPS - Linear containing 15% Glass Fiber, 25% Milled Glass. |
|||
Flexural Strength | 157 MPa | 22800 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-4240 PPS/PPA Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
Saint-Gobain Meldin® 3140 Thermoplastic Bearing Material Meldin 3140 is an ideal thrust washer material and is well suited for thrust washer applications. Its high strength and stiffness, combined with its excellent heat dissipation properties, make it a.. |
|||
Flexural Strength | 157 MPa | 22700 psi | ASTM D790 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Flexural Strength | 157 MPa | 22700 psi | ASTM D790 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Flexural Strength | 157 MPa | 22700 psi | ASTM D790 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Flexural Strength | 157 MPa | 22700 psi | ASTM D790 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Flexural Strength | 157 MPa | 22700 psi | ASTM D790 |
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Flexural Strength | 157 MPa | 22700 psi | ASTM D790 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Flexural Strength | 157 MPa | 22700 psi | ASTM D790 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 415 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 684 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Strength | 157 MPa | 22800 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 462 Glass/Mineral Reinforced, PET Alloy, Impact Modified, UL Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 157 MPa | 22800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6 LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |