Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 116 MPa | 16800 psi | |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Nilit Polynil® P60 Medium Viscosity Nylon 66 Description: Polynil P60 is a grade has a viscosity that has been optimized for monofilament extrusion.Key characteristics: Viscosity number 155 gr/cm3Excellent melt stabilityHigh elongationInformat.. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E.. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491.. |
|||
Flexural Strength | 116 MPa | 16800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4017 ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 116 MPa | 16800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4017 ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 116 MPa | 16800 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Techmer ES Luriblend® POM CO AF15 Availability: North AmericaForms: PelletsAdditive: Aramid Resin Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D638 |
Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Plenco 6401 Phenolic, Granular, Compression Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Flexural Strength | 116 MPa | 16800 psi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
Flexural Strength | 116 MPa | 16800 psi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
Flexural Strength | 116 MPa | 16800 psi | GB/9341 |
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 116 MPa | 16800 psi | ISO 178 |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced Information provided by Entec |
|||
Flexural Strength | 116 MPa | 16800 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GF3 POM 15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0153 30% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0570 30% Glass Fiber Reinforced, Flame Retardant Information provided by Asahi Thermofil |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Ashley Polymers Ashlene® N541 Nylon 66 A general purpose high viscosity extrusion grade Nylon 66 with very good natural color.Data provided by the manufacturer |
|||
Flexural Strength | 116 MPa | 16800 psi | ASTM D790 |
Ashley Polymers Ashlene® N541L Nylon 66 A general purpose injection molding grade for heavy parts.Data provided by the manufacturer |
|||
Flexural Strength | 116 - 143 MPa | 16800 - 20800 psi | |
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr.. |
|||
Flexural Strength | 116 MPa | 16800 psi | 2 mm/min; ISO 178 |
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000 PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me.. |