Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.71 MPa @Strain 120.38 %, Temperature 90.0 °C |
1410 psi @Strain 120.38 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.71 MPa @Strain 120.38 %, Temperature 90.0 °C |
1410 psi @Strain 120.38 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.74 MPa @Strain 17.77 %, Temperature 90.0 °C |
1410 psi @Strain 17.77 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.71 MPa @Strain 7.30 %, Temperature 120 °C |
1410 psi @Strain 7.30 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.70 MPa @Strain 10.0 % |
1410 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tensile Stress | 9.73 MPa @Strain 247.4 %, Temperature 120 °C |
1410 psi @Strain 247.4 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.73 MPa @Strain 0.220 %, Temperature -20.0 °C |
1410 psi @Strain 0.220 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.75 MPa @Strain 0.120 %, Temperature 120 °C |
1410 psi @Strain 0.120 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 9.69 MPa @Strain 33.67 %, Temperature 90.0 °C |
1410 psi @Strain 33.67 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 9.69 MPa @Strain 141.75 %, Temperature 150 °C |
1410 psi @Strain 141.75 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.69 MPa @Strain 33.67 %, Temperature 90.0 °C |
1410 psi @Strain 33.67 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.69 MPa @Strain 1.21 %, Temperature 90.0 °C |
1410 psi @Strain 1.21 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |