Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 84110 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by.. |
|||
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.71 J/cm @Temperature 23.0 °C |
10.7 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 5.70 J/cm @Temperature 23.0 °C |
10.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Izod Impact, Notched | 5.70 J/cm @Thickness 3.18 mm, Temperature -30.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 5.70 J/cm @Temperature -10.0 °C |
10.7 ft-lb/in @Temperature 14.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Izod Impact, Notched | >= 5.69 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 10.7 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5006B PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.69 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.69 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.69 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.71 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D-256 |
Axiall Suprel® 9422 Rigid PVC, Molding Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with.. |
|||
Izod Impact, Notched | 5.69 J/cm @Thickness 3.20 mm |
10.7 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Izod Impact, Notched | 5.70 J/cm @Temperature 23.0 °C |
10.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Izod Impact, Notched | 5.69 J/cm @Thickness 3.20 mm |
10.7 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |