Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.43 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87564 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 0.000 °C |
8.43 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
8.43 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.43 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Izod Impact, Notched | >= 4.50 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 8.43 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa LONOY 2100 LT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.43 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.17 mm |
8.43 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 2.4%); ASTM-D256 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 0.000 °C |
8.43 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 4500 T V0 Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE free, with halogens, high impact resistance, high thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 0.000 °C |
8.43 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 6500 F Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh melt flow rate, good thermal resistance, good impact resistance, excellent processability, good surface appearanceInformation provided by .. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 0.000 °C |
8.43 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 8500 Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND CR Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blend for chromium plating, painting and metallizationGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 0.000 °C |
8.43 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 2060 V0 Flame Retardant Polycarbonate Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 0.000 °C |
8.43 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 2060 V0 HF Flame Retardant Polycarbonate Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro.. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® TU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® TU 75 AV is a high melt flow rate, controlled rheology heterophasic copolymer with very high impact strength, even at low temperature. It contains antistatic and nucleating.. |