Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.12 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by.. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.12 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG704W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem.. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.12 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.12 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.12 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.12 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR407E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by.. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.17 mm |
3.12 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.17 mm |
3.12 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.35 mm |
3.12 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.35 mm |
3.12 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VS-0800 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.17 mm |
3.12 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0957 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.17 mm |
3.12 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.17 mm |
3.12 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.35 mm |
3.12 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.35 mm |
3.12 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VS-0800 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.67 J/cm @Temperature 23.0 °C |
3.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5211PBR High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Non pressure pipes, co-extruded pipes as the inner layerInformation provided by SCG Chemicals |
|||
Izod Impact, Notched | >= 1.67 J/cm @Temperature 23.0 °C |
>= 3.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chem.. |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm |
3.12 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm |
3.12 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm |
3.12 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade Medium Impact, High Gloss, High FlowInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm |
3.12 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm |
3.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm |
3.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM17V ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm |
3.12 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm |
3.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm |
3.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm |
3.12 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm |
3.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 6.40 mm |
3.12 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade Medium Impact, High Gloss, High FlowInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.67 J/cm @Thickness 3.20 mm |
3.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM17A TT ABS Injection Molding Grade High Flow, Medium ImpactInformation provided by Bhansali |