Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 37.0 J | 27.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Impact Test | 37.0 J | 27.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific) LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Impact Test | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl PX5622 PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da.. |
|||
Impact Test | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 37.0 J | 27.3 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Impact Test | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |
|||
Impact Test | 37.0 J | 27.3 ft-lb | HRC 65, unnotched |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
Impact Test | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |