Polymer Property : Impact Test = 37.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® EFX810ME PC
Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region.
Impact Test 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 37.0 J
27.3 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Colorcomp D10009 PC
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
Impact Test 37.0 J
27.3 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific)
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
Impact Test 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl PX5622 PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da..
Impact Test 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl RF1132 PPE+PP
PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region.
Impact Test 37.0 J
27.3 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Impact Test 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp MX01767C PP
LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB..
Impact Test 37.0 J
27.3 ft-lb
HRC 65, unnotched
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel
Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive..
Impact Test 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon MX01767C PP
LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB..