Mechanical Properties Metric English Comments
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolys..
300% Modulus 0.00800 GPa
1.16 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.00800 GPa
1.16 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.00800 GPa
1.16 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester
Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
300% Modulus 0.00800 GPa
1.16 ksi
DIN 53504
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
300% Modulus 0.00800 GPa
1.16 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr..
300% Modulus 0.00800 GPa
1.16 ksi
ISO 37
Huntsman AVALON® 80 AE Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
300% Modulus 0.00800 GPa
1.16 ksi
ISO 37
Huntsman AVALON® 80 AHT DP Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer
PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist..
300% Modulus 0.00800 GPa
1.16 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer
Description: Stat-Rite® E-1140 is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1140 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to ..
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.00800 GPa
1.16 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBTS
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
300% Modulus 0.00800 GPa
1.16 ksi
DIN 53504
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00800 GPa
1.16 ksi
DIN 53504
Lubrizol ESTANE® 58610 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00800 GPa
1.16 ksi
ISO 37
Lubrizol ESTANE® GP80AE Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00800 GPa
1.16 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.00800 GPa
1.16 ksi
DIN 53504
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D638
ELASTO UK Dryflex® 420351S SBS Based Material, 35D Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D638
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00800 GPa
1.16 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4640 Dense Extruded Profile
FormulationNordel® IP 4640
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.00800 GPa
1.16 ksi
Compounded, 35 mins.; ASTM D3185
Dynasol Solprene® 233 Medium CIS Polybutadiene
Solprene 233 is a medium cis polybutadiene used in applications where good performance at low temperatures and excellent abrasion resistance are needed. It is designed for critical processing applic..
300% Modulus 0.00800 GPa
1.16 ksi
DIN 53504
Lubrizol ESTANE® 54630 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00800 GPa
1.16 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBTS
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Copyright © lookpolymers.com All Rights Reserved