Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength 24.0 MPa
3480 psi
ASTM D412
Elongation at Break 560 %
560 %
ASTM D412
100% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Tear Strength 100 kN/m
571 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 180 - 200 °C
356 - 392 °F