Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 17.9 MPa | 2600 psi | alum/aluminum |
Resinlab® AR 4340 HP Metal Bonding Methacrylate Adhesive Resinlab™ AR 4340 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. It is an accelerated version.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | alum/aluminum |
Resinlab® AR 4400 HP Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | tensile shear; ASTM D1002 |
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive TRA-BOND 2248 is a thixotropic, high temperature cure, 100% solids epoxy resin system that provides strong, tough bonds between a wide range of materials (includes metals, glass, ceramics, and many .. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond F114BK01 Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114BK01 is a low viscosity, room temperature cure, epoxy system that contains no solvents, has excellent wicking and wetting characteristics, and adheres strongly to glass, ceramics, most .. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum, 2 hrs @ 65°C |
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy TRA-DUCT 916H01 is an electronically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical .. |
|||
Adhesive Bond Strength | >= 17.9 MPa | >= 2600 psi | after 30 days water absorption |
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum, @ 25°C |
Tra-Con Tra-Bond 968-5 High Dielectric Constant Epoxy Adhesive TRA-BOND 968-5 is a high dielectric constant epoxy adhesive. This one component, electrically insulating epoxy adhesive is designed for chip bonding.Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum, 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Grit blasted steel |
Loctite® 408 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Grit blasted steel |
Loctite® 455 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Grit blasted steel |
Loctite® 460 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 17.9 MPa @Temperature 82.2 °C |
2600 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-2/E Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st.. |
|||
Adhesive Bond Strength | 17.9 MPa | 2600 psi | Grit blasted steel |
Loctite® PRISM® 403 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |