Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® PRISM® 403 Instant Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name PRISM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® PRISM® 403 Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-specific, instant adhesives. Loctite® Instant Adhesives are available in a variety of viscosities, cure speeds, gap-filling capability and substrate compatibility. The ultra high-performance PRISM® family offers additional products that surpass the most stringent demands, including toughened formulations, low odor and low blooming products, surface insensitive and thermally resistant formulations.Loctite® 403 Low odor/low bloom Alkoxy PRISM® Instant AdhesiveAn adhesive for less-precisely fitted parts. Eliminates the need for sophisticated ventilation. Cure Type: 5084 Bonding Type: Cyanoacrylate Typical Use: Gap filling
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Viscosity 1000 cP
1000 cP
Mechanical Properties Metric English Comments
Adhesive Bond Strength 17.9 MPa
2600 psi
Grit blasted steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 0.830 min
0.0138 hour
1440 min
24.0 hour
Full Cure; Varies with substrates
Descriptive Properties Value Comments
Color Clear
Gap Fill 0.008 in.
Users viewing this material also viewed the following: