Polymer Property : Adhesive Bond Strength = 5.52 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.52 MPa
800 psi
Cast aluminum substrate 20 min @ 150°C (MT); ASTM D1002
Dow BETADAMP™ 32HT  (discontinued **)
BETADAMP™ 32HT is a high temperature vibration damper that can be applied to the exterior of cast aluminum or steel engine valve, transmission, and crankcase (oil pan) covers or electro-coat substr..
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
shear, Al/Al, after 30 days water immersion
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive
Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl..
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
shear, Al/Al, after 30 days water immersion
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy
Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl..
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
shear, Al/Al, after 30 days water immersion
Master Bond EP21TDCSMed Two Component, Silver Conductive USP Class VI Epoxy
Master Bond Polymer System EP21TDCS MED is a two component, silver filled, electrically conductive adhesive/sealant that meets USP Class VI specifications for medical applications. The high strength..
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
After 30 days water immersion
Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy
Master Bond Polymer System EP79 is a two component, silver coated, nickel filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or ..
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
After 30 days water immersion
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive
Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibilit..
Adhesive Bond Strength 5.52 MPa
800 psi
Lap shear, gold to gold, 45 min @ 150°C
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant
TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low..
Adhesive Bond Strength 5.52 MPa
800 psi
Lap shear, glass to glass
Tra-Con Tra-Coat WCC2A Clear Dual-Cure Semi-Flexible Adhesive
WCC2A is a clear, non-yellowing, dual-cure (UV and Heat) nameplate coating that is ideal for applications that require a glossy, "lens-like" finish. This photopolymer will also offer low shrinkage d..
Adhesive Bond Strength 5.52 MPa
800 psi
Trelleborg Emerson & Cuming Eccobond® 56C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Emerson & Cuming 56C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveSilver filled, high electrical conductivity, epoxy adhesive. Excellent thermal conductivity. Require..
Adhesive Bond Strength 5.52 MPa
800 psi
Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive
Emerson & Cuming 64C Eccobond® Two-Component Nickel Filled Electrically Conductive Epoxy AdhesiveTwo component, nickel filled, electrically conductive epoxy adhesive. Room temperature cure. Good ba..
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
shear, Al/Al, after 30 days water immersion
Master Bond EP21TDCSLO Two Component Silver Conductive Epoxy Adhesive
Master Bond Polymer System EP21TDCS-LO is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rap..
Adhesive Bond Strength 5.52 MPa
800 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy
TRA-DUCT 916D01 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr..
Adhesive Bond Strength 5.52 MPa

@Temperature 82.2 °C
800 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-12 Epoxy Adhesive, at 2:3 Mix Ratio
Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati..