Adhesive Bond Strength 17.9 MPa
2600 psi
alum/aluminum
Resinlab® AR 4340 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4340 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. It is an accelerated version..
Adhesive Bond Strength 17.9 MPa
2600 psi
alum/aluminum
Resinlab® AR 4400 HP Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a..
Adhesive Bond Strength 17.9 MPa
2600 psi
tensile shear; ASTM D1002
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum
Information provided by ITW Devcon
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive
TRA-BOND 2248 is a thixotropic, high temperature cure, 100% solids epoxy resin system that provides strong, tough bonds between a wide range of materials (includes metals, glass, ceramics, and many ..
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, 1 hr @ 65°C
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive
TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms..
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Tra-Con Tra-Bond F114BK01 Low Viscosity Blush-Free Epoxy Adhesive
TRA-BOND F114BK01 is a low viscosity, room temperature cure, epoxy system that contains no solvents, has excellent wicking and wetting characteristics, and adheres strongly to glass, ceramics, most ..
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound
TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical..
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, 1 hr @ 65°C
Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy
TRA-DUCT 916H01 is an electronically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical ..
Adhesive Bond Strength >= 17.9 MPa
>= 2600 psi
after 30 days water absorption
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System
Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings...
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, @ 25°C
Tra-Con Tra-Bond 968-5 High Dielectric Constant Epoxy Adhesive
TRA-BOND 968-5 is a high dielectric constant epoxy adhesive. This one component, electrically insulating epoxy adhesive is designed for chip bonding.Information provided by Tra-Con Inc.
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, 4 hrs @ 25°C + 2 hrs @ 65°C
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System
TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit..
Adhesive Bond Strength 17.9 MPa
2600 psi
Grit blasted steel
Loctite® 408 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 17.9 MPa
2600 psi
Grit blasted steel
Loctite® 455 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 17.9 MPa
2600 psi
Grit blasted steel
Loctite® 460 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 17.9 MPa

@Temperature 82.2 °C
2600 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-2/E Epoxy Adhesive
This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac..
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st..
Adhesive Bond Strength 17.9 MPa
2600 psi
Grit blasted steel
Loctite® PRISM® 403 Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..