Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |