Polymer Property : Modulus of Elasticity = 3.20 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.20 GPa
464 ksi
ASTM D638
Plaskolite Optix® CA-71 General Purpose Acrylic Resin
Injection Molding and Extrusion Grade Pellets. High heat resistance, medium flow.
Modulus of Elasticity 3.20 GPa
464 ksi
50% RH
Murtfeldt Murylon® A GF Nylon 66, Glass Reinforced
Murylon® A’s impressive characteristics are enhanced with admixed glass fibers. This results in a clear improvement in cold flow behavior and dimensional stability, enabling higher static pressure..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 178
Premix Thermoplastics PRE-ELEC® PP 1378
PRE-ELEC PP 1378 is a conductive thermoplastic compound based on glass-fiber reinforced polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electri..
Modulus of Elasticity 3.20 - 3.50 GPa
464 - 508 ksi
ASTM D638-04
Proto3000 Objet RGD525 High Temperature Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
Modulus of Elasticity 3.20 GPa
464 ksi
ASTM D638
Plaskolite West Optix® CA-71 General Purpose Acrylic Resin
Injection Molding and Extrusion Grade Pellets. High heat resistance, medium flow.
Modulus of Elasticity 3.20 - 4.30 GPa

@Temperature 60.0 - 120 °C
464 - 624 ksi

@Temperature 140 - 248 °F
Average value: 3.70 GPa Grade Count:1
Overview of materials for Polyphenylene Ether, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu..
Modulus of Elasticity 3.20 GPa
464 ksi
Plain Cast Resin; ASTM D638
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Modulus of Elasticity 3.20 GPa
464 ksi
DIN 53 457
Albis Plastics Tedur® L V 9900-1 PPS, Unreinforced  (discontinued **)
Excellent Surface Finish, High Chemical Resistance. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pipes, ProfilesProcessing: Extrusion (Melt Temperature: 555-610°F)..
Modulus of Elasticity 3.20 GPa
464 ksi
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Conditioned
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527
GEHR Plastics PEI Polyetherimide
Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic..
Modulus of Elasticity 3.20 GPa
464 ksi
Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Global EPP PA 6C IMPACT Cast Polyamide 6 + Plasticizer
Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of ..
Modulus of Elasticity 3.20 GPa

@Temperature 25.0 °C
464 ksi

@Temperature 77.0 °F
Storage
Lord Adhesives Thermosetâ„¢ MD-110 Conductive Adhesive
LORD Thermosetâ„¢ MD-110 silver-filled conductive adhesive offers excellent electrical conductivity and room temperature stability. It is designed for use with automated dispensing, stamping and..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527-2
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Modulus of Elasticity 3.20 GPa
464 ksi
Plain Cast Resin; ASTM D638
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Modulus of Elasticity 3.20 GPa
464 ksi
TD; ExxonMobil Method
ExxonMobil Oppalyte™ 35MD447 OPP Film
Product Description: A coextruded super white opaque, modified high density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527-1/-2
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527-1/-2
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527-1/-2
BASF Ultramid® KR 4350 PA6/6T (Conditioned)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527-1/-2
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527-1/-2
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned)
Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain..
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 178
Addiplast Addilene H 442 M30 Polypropylene Homopolymer
High heat resistance, detergent stabilizedInformation provided by Addiplast.
Modulus of Elasticity 3.20 GPa
464 ksi
TD; ExxonMobil Method
ExxonMobil Oppalyte™ 30MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..
Modulus of Elasticity 3.20 GPa
464 ksi
TD; ExxonMobil Method
ExxonMobil Oppalyte™ 40MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..
Modulus of Elasticity 3.20 - 14.0 GPa
464 - 2030 ksi
Average value: 5.74 GPa Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Modulus of Elasticity 3.20 GPa
464 ksi
Lehmann & Voss PLASLUBE NY-1/SI/2/NT Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann ..