Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.20 GPa | 319 ksi | ASTM D638 |
Network Polymers MS 150 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Modulus of Elasticity | 2.20 - 6.48 GPa | 319 - 940 ksi | Average value: 4.10 GPa Grade Count:62 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Modulus of Elasticity | 2.20 - 5.60 GPa | 319 - 812 ksi | Average value: 3.24 GPa Grade Count:5 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | DIN 53457 |
Ineos Nova S-4400 High Impact Compact Polystyrene
(discontinued **) Impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical parts o.. |
|||
Modulus of Elasticity | 2.20 - 6.00 GPa @Temperature 60.0 - 120 °C |
319 - 870 ksi @Temperature 140 - 248 °F |
Average value: 4.02 GPa Grade Count:2 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 2.20 - 14.5 GPa | 319 - 2100 ksi | Average value: 7.24 GPa Grade Count:14 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50-0957 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80-7318 Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80-8318-1 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 527 |
GEHR Plastics POM-10PE Acetal Copolymer Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 0104 Polycarbonate Suitable for extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 1218 Polycarbonate Suitable for molding, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 3859 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 5970 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 0712 Polycarbonate Suitable for molding and extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 2230 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ASTM D638 |
Spartech Royalite R60M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. This rigid, fire-rated, proprietary resin is specifically formulated to meet the requirements of the FAR 25.853 A flammability test. Primary applications are air.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 21MBT621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 32MB600 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 178 |
Addiplast Addilene J 120 M20 Polypropylene Copolymer Low fluidity for extrusion or injectionInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2 K20 Nylon 6 High density and high modulusInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 527-2 |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | Conditioned; ISO 178 |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.20 - 3.45 GPa | 319 - 501 ksi | Average value: 2.96 GPa Grade Count:6 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |