Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 3.45 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.21 - 3.45 GPa
320 - 500 ksi
Average value: 2.81 GPa Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
Modulus of Elasticity 1.10 - 3.45 GPa
160 - 500 ksi
Average value: 2.19 GPa Grade Count:85
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Modulus of Elasticity 1.79 - 3.45 GPa
260 - 500 ksi
Average value: 2.77 GPa Grade Count:9
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 1.38 - 3.45 GPa
200 - 500 ksi
Average value: 2.16 GPa Grade Count:23
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
Modulus of Elasticity 2.20 - 3.45 GPa
319 - 501 ksi
Average value: 2.96 GPa Grade Count:6
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max..
Modulus of Elasticity 0.000138 - 3.45 GPa
0.0200 - 500 ksi
Average value: 1.39 GPa Grade Count:36
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
Copyright © lookpolymers.com All Rights Reserved