Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Modulus of Elasticity | 2.10 - 8.27 GPa | 305 - 1200 ksi | Average value: 5.57 GPa Grade Count:57 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Modulus of Elasticity | 2.10 - 7.20 GPa @Temperature 60.0 - 150 °C |
305 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 4.28 GPa Grade Count:3 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ASTM D638 |
Spartech Royalite R61M Low Smoke Resin Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 33LL247 OPP Film Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LTL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired. 47LTL247 with supplied .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50ML580 OPP Film Product Description: A metalized, surface printable OPP film designed for pressure sensitive applications where high-sheen metalized appearance and high-speed press performance are desired. The prop.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 38MW280 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side. Ideal for single web packaging applications on HFFS in combination with cold seal.Availability.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW648 OPP Film Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38ICE OPP Film Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38MO447 OPP Film Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film, heat sealable on the inside. The treated layer must be printed and varnished to provide the necess.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene H 555 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene PMD 50213 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addinyl B2 R Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addinyl PMD 20143 Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 33MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW647 OPP Film Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene H 552 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |