Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IDI Composites 46-12 Thermoset Polyester, Molding

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer IDI Composites
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF IDI Composites 46-12 Thermoset Polyester, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Highest strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Water Absorption 0.15 %
0.15 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 35 - 45
35 - 45
ASTM D2583
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Flexural Strength 141 MPa
20500 psi
ASTM D790
Compressive Strength 159 MPa
23100 psi
ASTM D695
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495