Mechanical Properties Metric English Comments
Compressive Strength >= 12.0 MPa
>= 1740 psi
Parallel to holes
MarkeTech H-2 Honeycomb Ceramic
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo..
Compressive Strength >= 12.0 MPa
>= 1740 psi
Parallel to holes
MarkeTech H-3 Honeycomb Ceramic
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo..
Compressive Strength >= 12.0 MPa
>= 1740 psi
Parallel to holes
MarkeTech H-4 Honeycomb Ceramic
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo..
Compressive Strength 12.0 - 18.0 MPa
1740 - 2610 psi
Cold Crushing Strength
Gouda Vuurvast FI 25-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 12.0 - 18.0 MPa
1740 - 2610 psi
Cold Crushing Strength
Gouda Vuurvast FI 35-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 12.0 - 18.0 MPa
1740 - 2610 psi
Cold Crushing Strength
Gouda Vuurvast FI 45-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 12.0 MPa

@Time 360000 sec
1740 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Compressive Strength 12.0 MPa

@Time 360000 sec
1740 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
Compressive Strength 12.0 - 16.0 MPa
1740 - 2320 psi
Cold Crushing Strength
Gouda Vuurvast FI 25-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 12.0 - 16.0 MPa
1740 - 2320 psi
Cold Crushing Strength
Gouda Vuurvast FI 35-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength >= 12.0 MPa

@Temperature 23.0 °C,
Time 86400 sec
>= 1740 psi

@Temperature 73.4 °F,
Time 24.0 hour
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621
Adamas Adalon® 305 PTFE, 15% Graphite