Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 100 MPa | 14500 psi | Type B, 5mm/min; ISO 604:2002 |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PET PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast AK 85 P1 Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. In order to optimized the resistance against aluminum attack the sum of Al2O.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast AK 94 M Dense Refractory Brick Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast LP 60 AAP Dense Refractory Brick Description: Special low porosity quality for use under severe corrosive conditions, (for instance liquid slags). Moreover, this brick has been extra protected against slag attack because it also co.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast LP 85 AM Dense Refractory Brick Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron lad.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast AK 85 PW Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average.. |
|||
Compressive Strength | 100 MPa | 14500 psi | |
SGL Carbon Group EK 40 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 100 MPa | 14500 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Compressive Strength | 100 - 300 MPa | 14500 - 43500 psi | Longitudinal |
Goodfellow Polyaramid/Vinylester Composite Tube or Rod Information provided by Goodfellow. |
|||
Compressive Strength | 100 MPa | 14500 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 23 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Very coarse weave ( |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 32 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 33 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Very coarse weave ( |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 34 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CP 23 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal and high relative humidity.Information provided by Hippe. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CP 32 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity. Improved mechanical and electrical properties when compared to PF .. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Ambient |
China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Compressive Strength | 100 MPa | 14500 psi | EN ISO 604 |
Brandenburger S 2000 A Side Insulation S 2000 A is reinforced with load-bearing glass fibre mat with thermoset weave. A laminated aluminum lining provides additional heat-reflecting protection.Information provided by Brandenburger Isolie.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast LP 60 M Dense Refractory Brick Description: LP 60 M is a special low porosity, high strength material based on raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a ma.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast LP 97-3 Dense Refractory Brick Description: A high alumina quality brick containing a limited percentage of chromium oxide for improved slag resistance. The product has a very low silica- and iron oxide percentage so that it can .. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast SiC 90 Dense Refractory Brick Description: Very good thermal shock resistance, abrasion resistance as well as very good heat conductivity makes this SiC based brick very well suited for muffles as well as for applications under .. |