Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer China-Yixing Longly Refractories Co. Ltd
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum mullite) high erosion-resistant, anti-erosion; high-temperature conditions, particularly excellent cross-bending and anti-broken; efficient thermal conductivity and mechanical load power, chemical stability, performance, good thermal shock resistance, excellent creep resistance, long service life; more cost-effective, is the preferred burning kiln furniture for electronic kiln of firing process. Widely used in chemical, ceramics, electronic and magnetic materials of high-temperature furnace.Application: Magnetic materials, electronic ceramics.Information Provided by China Yixing Longly Refractories Co. Ltd
Physical Properties Metric English Comments
Bulk Density >= 2.80 g/cc
>= 0.101 lb/in³
Porosity >= 18 %
>= 18 %
Apparent
Mechanical Properties Metric English Comments
Flexural Strength >= 29.0 MPa
>= 4210 psi
high temp bending
>= 110 MPa
>= 16000 psi
cold bending
Compressive Strength >= 100 MPa
>= 14500 psi
Ambient
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 1750 °C
>= 3180 °F
Component Elements Properties Metric English Comments
Al2O3 >= 86.8 %
>= 86.8 %
Fe2O3 <= 0.080 %
<= 0.080 %
SiO2 <= 9.1 %
<= 9.1 %
Descriptive Properties Value Comments
Refractoriness (°C) >1700
Under load temperature, 0.2 MPa, 0.6%