Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 152 MPa @Temperature 23.9 °C |
22000 psi @Temperature 75.0 °F |
Dry; 18oz. Woven roving form; ASTM D695 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, Glass Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Compressive Strength | 152 MPa @Temperature 93.3 °C |
22000 psi @Temperature 200 °F |
Dry; Post-Cure; ASTM D695 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Compressive Strength | 152 MPa | 22000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Quantum PEI - Ultem® Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
PolyOne Edgetek® PS-30GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Compressive Strength | 152 MPa | 22000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet) |
|||
Compressive Strength | 152 MPa | 22000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Plenco 4304 Phenolic, Nodular, Injection Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK) TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels.. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex.. |
|||
Compressive Strength | 152 - 172 MPa | 22000 - 25000 psi | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Compressive Strength | 152 - 200 MPa | 22000 - 29000 psi | |
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better .. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Compressive Strength | 152 - 165 MPa | 22000 - 24000 psi | |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Compressive Strength | 152 MPa | 22000 psi | Ultimate; TM R050-38 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Sumitomo Bakelite North America FS-10-VO-200-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound with excellent heat resistance.Meets the requirements of ASTM D5948 Type SIG-F.Information provided by Vyncolit.. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Resinoid 2018 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |