Lucite International Elvacite ® 2044 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2044 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elvacite® 2044 is a high molecular weight n-butyl methacrylate polymer. Elvacite® 2044 is useful in adhesives for smooth plastic films and aluminum, and in silk screen inks. It will plasticize and improve adhesion of harder butyl grades (Elvacite® 2045 and 2046) and nitrocellulose. Elvacite® 2044 can also be used to improve the outdoor durability of vinyl chloride resins in pigmented lacquers.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Viscosity Measurement 0.47 - 0.56
0.47 - 0.56
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 142000 g/mol
142000 g/mol
Mechanical Properties Metric English Comments
Hardness, Knoop 1.0
1.0
Tukon Hardness
Tensile Strength 3.45 MPa
500 psi
Elongation at Break 300 %
300 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Processing Properties Metric English Comments
Moisture Content 0.30 %
0.30 %