Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 130 MPa | 18900 psi | at Break (NYP); ISO 527-1/-2 |
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data) Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic.. |
|||
Tensile Strength | 130 MPa | 18900 psi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Strength | 130 MPa | 18900 psi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Strength | 130 MPa | 18900 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hGR20 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tensile Strength | 130 MPa | 18900 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F4MW4 Nylon 6, 40% Glass Fiber and Mineral Reinforced SAXAMID 126F4MW4 is a 40% glass fibers/ mineral reinforced polyamide 6 injection-molding-grade. It has dimensional stability and high strength.Information provided by SAX Polymers |
|||
Tensile Strength | 130 MPa | 18900 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers |
|||
Tensile Strength | 130 MPa @Thickness >=1.50 mm |
18900 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6 |
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr.. |
|||
Tensile Strength | 130 MPa | 18900 psi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Tensile Strength | 130 MPa | 18900 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Strength | 130 MPa | 18900 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Tensile Strength | 130 MPa | 18900 psi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Tensile Strength | 130 MPa | 18900 psi | ASTM D 638 |
Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material Meldin 1277 has structural integrity and low deformation. This material also exhibits good electrical insulative properties and dimensional stability.Meldin® 1000 series components are used in app.. |
|||
Tensile Strength | 130 MPa @Thickness >=1.50 mm |
18900 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6 |
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mecha.. |