Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Meldin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Meldin 1277 has structural integrity and low deformation. This material also exhibits good electrical insulative properties and dimensional stability.Meldin® 1000 series components are used in appliance applications due to their superior wear life and ability to operate without the need for any oils or lubricants. For scroll tip seal applications, Meldin® 1000 series materials provide some parts with superior wear resistance properties, and superior deformation properties over those of standard PTFE scroll tip seals. In vehicle systems such as transmission bearings or thrust washers, as well as fuel pump bearings, Meldin® 1000 series materials provide performance superior to metallic components. The Meldin 1000 series materials' wear resistance, coupled with their excellent chemical resistance, make them ideal materials for vehicle system components.
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
ASTM D793
Water Absorption 0.010 %
0.010 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 130 MPa
18900 psi
ASTM D 638
Elongation at Break 0.50 %
0.50 %
ASTM D 638
Flexural Strength 170 MPa
24700 psi
ASTM D 790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 2.50 µm/m-°C
1.39 µin/in-°F
ASTM E831-93
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
450 °F
ASTM D648