Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 70.0 - 390 MPa | 10200 - 56600 psi | MD |
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co.. |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Quantum Polysulfone Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Injection; ISO 527 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or .. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | DIN 53455 |
Isoflon POM H Polyacetal H Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | ISO 527 |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
Tensile Strength | 70.0 MPa | 10200 psi | ISO 527 |
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU) Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate.. |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU) Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr.. |
|||
Tensile Strength | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA/PP 7500 GF 7/1 Polyamide/Polypropylene Medium viscosity special compound with increased rigidity and low moisture absorption.Application: For molding parts with high mechanical requirements at low moisture absorption.Information provide.. |
|||
Tensile Strength | 70.0 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe PF CP 206 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe UP GM 201 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 CFHI Polyamide 6 - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | 50 mm/min; ISO 37 |
BASF Elastollan R 2002 25% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |
|||
Tensile Strength | 70.0 - 100 MPa | 10200 - 14500 psi | Compression; ISO 527 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Compression; ISO 527 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | DIN 53455 |
Isoflon PA 6 Polyamide 6 General use for mechanical partsGood heat resistanceEasy to useHigh moisture regainInformation provided by Isoflon. |