Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.58 MPa | 1100 psi | ASTM D638 |
Quadrant EPP Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet) |
|||
Tensile Strength | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 86479 Natural Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 86479 Opaque Polyvinyl Chloride Information provided by PolyOne |
|||
Tensile Strength | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 86479 Tran Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 30300R062 0.062" (1.57 mm) Uncured Silicone Rubber on Kodacel Carrier Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberCarrier: KodacelAppearance: Red silicone gum on polymer linersThis data represents typical values for the production mate.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 41300R062 0.062" Uncured Silicone Rubber on Holland Cloth Design/Construction:Interleave: 3.0 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Holland ClothThis data represents typical values for the production material and should not be used as m.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 55572XA028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Side 2 Silicone Property; ASTM D412 |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Side 2, Layer 2; Compound Property; ASTM D412 |
Arlon 55578R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Silicone Skim Coat Appearance: Red silico.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Side 1, Layer 2; Compound Property; ASTM D412 |
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber (Skim Coat).. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Layer 1, Silicone Property; ASTM D412 |
Arlon 55579R031H 0.0315" (0.800 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPELayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. T.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Layer 1, Silicone Property; ASTM D412 |
Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 55579XA028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material an.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Layer 2 Silicone Property; ASTM D412 |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 66211A007 0.007" (0.178 mm) Uncured Silicone Rubber Monofilament Polyester Fabric Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Monofilament Polyester Fabric Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represent.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 99570R010 0.010" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon LW201B##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon LW201B##-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon LW401Y##-M1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Yellow, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll lengt.. |
|||
Tensile Strength | >= 7.58 MPa | >= 1100 psi | Compound Property |
Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | ASTM D412 |
Aaron Industries AAROPRENE® ATPR 1000 80A Elastomeric Compound AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 44571XB015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate) Side 2: Uncured Silicone RubberInterleave: 2.5 mil .. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon 55572R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; Arlon SQA-TMS-008 |
Arlon 32570XA020 0.020" Uncured Silicone Rubber on Polyester Film Carrier Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |
|||
Tensile Strength | 7.58 MPa | 1100 psi | Silicone Property; ASTM D412 |
Arlon R36461R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Liner: Polyethylene This data represents typical values for.. |