| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 74 | 74 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 15.9 MPa | 2310 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 350 % | 350 % | 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -31.7 °C | -25.1 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
| 182 - 188 °C | 360 - 370 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | NSF 51 | GRAY 2600, BLACK 2999. Max. Temp. of use = 100 degrees F. |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Profile Extrusion | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Profiles |