Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible K85 Natural & Black Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2170G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2170G is a 70 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2170G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8001 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa | 901 psi | BAM 1211 |
Kraton® G1651 H (SEBS) Linear Triblock Copolymer Description: Kraton G1651 H is a clear, linear copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Compound Property |
Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications... |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 28601M015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Tan gum on glass fiber fabricThis data represents typical values for the production material. The data .. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Silicone Property |
Arlon 30400R060 0.06" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51571R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene Appearance: Black silicone gum on fiberglass clothThis da.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 1 Silicone Property; ASTM D412 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 2 Silicone Property; ASTM D412 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 56581R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon P29609R025 0.025" (0.635 mm) Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 1, Silicone Property; ASTM D412 |
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Compound Property; ASTM D412 |
Arlon 31570R020 0.020" (0.508 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the pr.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41580B030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 41600R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property |
Arlon 51581R018 0.018" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property, Side 1; ASTM D412 |
Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Rubber Appearance: Gray gum on glass fiber fabricThis data represe.. |
|||
Tensile Strength | 6.21 - 7.58 MPa | 900 - 1100 psi | Compound Property |
Arlon 44250R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Tensile Strength | 6.21 MPa | 900 psi | Silicone Property; ASTM D412 |
Arlon 47568R0055E 0.0075" (0.190 mm) Cured Silicone Rubber/Acrylic PSA Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 2113 FiberglassSide 2: Acrylic PSA Interleave: Polypropylene This data represents typical values for the production material. The.. |
|||
Tensile Strength | >= 6.21 MPa | >= 900 psi | Compound Property |
Arlon 30600R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Release Carrier Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis.. |