PolyOne Geon™ HC 2170G Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ HC 2170G Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Geon HC 2170G is a 70 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2170G can be used for extrusion and injection molding healthcare applications.NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application. This product is not recommended for long-term storage of blood or blood components. Please contact PolyOne for more information.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
15 sec; ASTM D2240
Tensile Strength at Break 15.9 MPa
2310 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 6.21 MPa

@Strain 100 %
901 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 480 %
480 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -31.7 °C
-25.1 °F
ASTM D746
Descriptive Properties Value Comments
Agency Ratings FDA Unspecified Rating
Appearance Clear - Blue Tint
Features BPA Free
Ethylene Oxide Sterilizable
Good Processability
High Clarity
Non-Phthalate Plasticizer
Radiation (Gamma) Resistant
Radiation Sterilizable
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Connectors
Disposable Hospital Goods
Hospital Goods
Medical Appliances
Medical/Healthcare Applications
Personal Care
Tubing