Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Melt Flow | 2.2 g/10 min @Load 21.6 kg, Temperature 190 °C |
2.2 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) BL7 HM 6255 High Density Polyethylene BL7 (HM 6255) is a high density polyethylene with Butene-1 as comonomer. It is a special grade for particularly high requirements like low temperature impact strength and stacking, good stress crack.. |
|||
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ISO 1133 |
Styron Magnumâ„¢ 3416 SC Natural Plus ABS Resin The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with sable light base color that is ideal for self-coloring.Information provided by Do.. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BL2631 High Density Polyethylene BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film Borclean HB311BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HB311BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved ProcessingDelrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100P provides maximum toughness in the product line.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met.. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3500 Natural 1050 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 4107 Heat Resistant Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 4500R Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |