Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Melt Flow | 14.5 g/10 min @Load 10.0 kg, Temperature 230 °C |
14.5 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM-D1238 |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Melt Flow | 14.5 g/10 min @Load 5.00 kg, Temperature 210 °C |
14.5 g/10 min @Load 11.0 lb, Temperature 410 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Melt Flow | 14.5 g/10 min @Load 5.00 kg, Temperature 210 °C |
14.5 g/10 min @Load 11.0 lb, Temperature 410 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Melt Flow | 14.5 g/10 min @Load 21.60 kg, Temperature 190 °C |
14.5 g/10 min @Load 47.62 lb, Temperature 374 °F |
ISO 1133 |
Total MDPE HF 513 Medium Density Polyethylene, Blown Film MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanic.. |
|||
Melt Flow | 14.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
14.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS VP-11 SHF Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |