Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 190 °C |
14 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding Eraclene MM 84 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 is characterized by high rigidity and good impact resistance. .. |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® BDT5510 ABS Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only. |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 190 °C |
14 g/10 min @Load 8.38 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged.. |
|||
Melt Flow | 14 - 18 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 - 18 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4223V (23416) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 14 - 42 g/10 min @Load 21.6 kg, Temperature 190 °C |
14 - 42 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT 15-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | >= 14 g/10 min @Load 5.00 kg, Temperature 190 °C |
>= 14 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
MTM Plastics Dipolen® SP Recycled PP Blend Dipolen® SP is a granulated polypropylene with other polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to custo.. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1500 PC PC1500 resin is a medium-high flow (MFR = 15 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 360 °C |
14 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 230 °C |
14 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borclean™ HC312BF Polypropylene Homopolymer for Capacitor Film Borclean HC312BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC312BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 10 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 260 °C |
14 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
JIS K 6719 |
Zeon Chemicals Zeonor® 1060R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Melt Flow | 14 g/10 min @Load 21.6 kg, Temperature 190 °C |
14 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Total MDPE HT 514 Medium Density Polyethylene, Blown Film MDPE HT 514 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HT 514 is a semi-high molecular weight polyethylene giving excellent mechanic.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 240 °C |
14 g/10 min @Load 11.0 lb, Temperature 464 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good light resistance, good processability and surface appearanceInformation provided by Cossa Polimeri S.. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Chi Mei Kibisan® PN-117 SAN Injection Molding |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 240 °C |
14 g/10 min @Load 4.76 lb, Temperature 464 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TWP 155 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 240 °C |
14 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 240 °C |
14 g/10 min @Load 4.76 lb, Temperature 464 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 190 °C |
14 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East) CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha.. |