Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPP 908 Description: Polyester CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1385 PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7980-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft T.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238(G) |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Melt Flow | <= 3.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
<= 3.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
MTM Plastics Purpolen® PE Polyethylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS 1950 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 2100 P Compounding Grade Powder Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 3500 HF Injection Molding Grade, High Flow, Medium Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3501 GF-30 Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3502E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 4003HH Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 9502E Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers NPP 60-908 Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers SAN 268 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 - 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 - 5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |